PCTG 韩国SK JN200注塑级
物性表
性能项目 | 测试条件 | 测试方法 | 数值/描述 | 单位 | |
机械性能 | 拉伸强度(引张强度) | ASTM D638/ISO527 | kg/cm²(MPa)[Lb/in2] | ||
断裂伸长率 | ASTM D638/ISO527 | 340 | % | ||
拉伸模量 | ASTM D638/ISO527 | kg/cm²(MPa)[Lb/in2] | |||
拉伸屈服伸长率(延伸率) | ASTM D638/ISO527 | % | |||
拉伸断裂伸长率(延伸率) | ASTM D638/ISO527 | % | |||
弯曲模量(弯曲弹性率) | ASTM D790/ISO178 | 18348 | kg/cm²(MPa)[Lb/in2] | ||
弯曲强度 | ASTM D790/ISO178 | 683 | kg/cm²(MPa)[Lb/in2] | ||
洛氏硬度 | ASTMD785 | 105 | |||
IZOD 缺口冲击强度 | 1/4" 23℃ | ASTM D256/ISO179 | kg·cm/cm(J/M)ft·lb/in | ||
1/4"-30℃ | ASTM D256/ISO179 | kg·cm/cm(J/M)ft·lb/in | |||
1/8" 23℃ | ASTM D256/ISO179 | kg·cm/cm(J/M)ft·lb/in | |||
1/8"-30℃ | ASTM D256/ISO179 | kg·cm/cm(J/M)ft·lb/in | |||
Charpy冲击强度 | 23℃ (缺口) | ASTM D256/ISO179 | kg·cm/cm(J/M)ft·lb/in | ||
-30℃(缺口) | ASTM D256/ISO179 | kg·cm/cm(J/M)ft·lb/in | |||
23℃(无缺口) | ASTM D256/ISO179 | kg·cm/cm(J/M)ft·lb/in | |||
-30℃(无缺口) | ASTM D256/ISO179 | kg·cm/cm(J/M)ft·lb/in |